dc.description.abstractSintesis film tipis BaTiO3 dengan variasi konsentrasi pendadah Fe (0%; 2%; 4%; dan 6%) menggunakan metode chemical solution deposition (CSD) berhasil dilakukan. Larutan sampel dideposisikan di atas substrat silikon (100) tipe-p dengan teknik spin coating pada kecepatan anguler 8000 rpm selama 60 detik. Proses annealing dimulai pada suhu kamar hingga mencapai suhu 850°C dan ditahan selama 8 jam dengan kelajuan suhu sebesar 1,67°C/menit, dilanjutkan dengan pendinginan hingga suhu kamar selama 12 jam. Ketebalan film dihitung dengan metode volumetrik dan hasilnya berturut-turut yaitu 3,9867 μm; 3,8759 μm; 3,6913 μm; dan 3,0454 μm. Analisis dengan persamaan Cramer-Cohen menghasilkan parameter kisi a = b yaitu 3,843 Å; 3,882 Å; 3,898 Å; dan 3,909 Å serta parameter kisi c yaitu 4,002 Å; 3,938 Å; 4,070 Å; dan 4,024 Å dengan struktur kristal tetragonal. Nilai enegi band gap hasil analisis dengan fungsi Kubelka Munk untuk indirect transition berada dalam rentang 3,0689 – 3,2051 eV dan direct transition berada dalam rentang 2,7660 – 3,0417 eV.id
dc.description.abstractThe synthesis of BaTiO3 thin film with variations in concentration of Fe as dopant (0%; 2%; 4%; and 6%) using chemical solution deposition (CSD) method has been successfully done. The solutions was deposited on p-type silicon (100) substrates with spin coating technique at the angular speed of 8000 rpm for 60 seconds. The annealing process was started at room temperature until 850°C and was held for 8 hours with a temperature speed of 1.67°C/minutes, followed by cooling process to room temperature for 12 hours. Film thickness was calculated using volumetric method and the results are 3.9867 μm; 3.8759 μm; 3.6913 μm; and 3.0454 μm. The results of the analysis using Cramer-Cohen equation obtained that the lattice parameters a = b are 3.843 Å; 3.882 Å; 3.898 Å; and 3.909 Å and c are 4.002 Å; 3.938 Å; 4.070 Å; and 4.024 Å with tetragonal crystal structure. The values of band gap energy that was analyzed using Kubelka-Munk method equation are in range of 3.0689 – 3.2051 eV for indirect transition and 2.7660 – 3.0417 eV for direct transition.id
dc.language.isoidid
dc.publisherIPB Universityid
dc.titleSintesis dan Uji Sifat Film Tipis Barium Titanat (BaTiO3) dengan Variasi Konsentrasi Iron (II) Asetat (Fe(CH3COO)2) sebagai Pendadahid
dc.title.alternativeSynthesis and Characterizations of Barium Titanate (BaTiO3) Thin Film with Varied Concentration of Iron (II) Acetate (Fe(CH3COO)2) as Dopantid
dc.typeUndergraduate Thesisid
dc.subject.keywordthin filmid
dc.subject.keywordbarium titanateid
dc.subject.keywordcramer-cohenid
dc.subject.keywordkubelka-munkid
dc.subject.keyworddopantid


Files in this item

Thumbnail
Thumbnail
Thumbnail

This item appears in the following Collection(s)

Show simple item record