      Penentuan Waktu Oksidasi Terbaik untuk Proses Penyamakan Kulit Samoa Menggunakan Minyak Biji Karet dengan Oksidator Natrium Hipoklorit

      Thumbnail
      View/Open
      Abstract (294.0Kb)
      Bab I (296.1Kb)
      Bab II (468.8Kb)
      Bab III (362.3Kb)
      Bab IV (581.1Kb)
      Bab V (294.3Kb)
      Cover (316.4Kb)
      Daftar Pustaka (308.4Kb)
      Full text (1.625Mb)
      Lampiran (1.082Mb)
      Date
      2011
      Author
      Febianti, Irfina
      Suparno,Ono
      Metadata
      Show full item record
      Abstract
      Chamois leather is a well known product, as it has specific uses for gasoline filtration, cleaning and drying of optical equipment, spectacles, mirror and vehicles. It can be produced by using rubber seed oil and oxidizing agent of sodium hypochlorite. The best oxidation time condition for tanning need to be applied in order to obtain good quality leather. The objectives of the research was to determine the best oxidation time condition for the tanning process. The experiment was carried out by tanning of goat pickle pelts for 4, 6, 8 hours of oxidation times inside the rotary drum and 1, 2, 3 days of oxidation times at a toggle dryer. This study shows that the chemical, physical and organoleptic properties of the leather met the quality requirements for the chamois leather. The best oxidation times for the process were 4 hours in the rotary drum and hang at toggle for 3 days. The chemical properties of the leathers were pH of 7.48, ash content of 1.99%, and oil content of 4.51%. Their physical properties were thickness of 0.7 mm, tensile strength of 30.20 N/mm2, elongation at break 178.09%, tear strength of 75.105 N/mm, and water absorption of 315.655% (2 hours) and 346.49% (24 hours). The organoleptic properties of the leathers, i.e. softness, colour and odour, were considered good to excellent.
      URI
      http://repository.ipb.ac.id/handle/123456789/53029
      Collections
      • UT - Agroindustrial Technology [4352]

      Copyright © 2020 Library of IPB University
      All rights reserved
      Contact Us | Send Feedback
      Indonesia DSpace Group 
      IPB University Scientific Repository
      UIN Syarif Hidayatullah Institutional Repository
      Universitas Jember Digital Repository
        

       

      Browse

      All of IPB RepositoryCollectionsBy Issue DateAuthorsTitlesSubjectsThis CollectionBy Issue DateAuthorsTitlesSubjects

      My Account

      Login

      Application

      google store

      Copyright © 2020 Library of IPB University
      All rights reserved
      Contact Us | Send Feedback
      Indonesia DSpace Group 
      IPB University Scientific Repository
      UIN Syarif Hidayatullah Institutional Repository
      Universitas Jember Digital Repository