http://repository.ipb.ac.id/handle/123456789/109750| Title: | Pembuatan Film Tipis BaxSr1-xTiO3 dengan Variasi Fraksi Mol (x = 0; 0,125; 0,250; 0,375) Menggunakan Metode Chemical Solution Deposition |
| Authors: | Zuhri, Mahfuddin Irzaman Ni'mah, Rizkiyah Khairun |
| Issue Date: | 2021 |
| Publisher: | IPB University |
| Abstract: | Pembuatan film tipis BaxSr1-xTiO3 dengan variasi fraksi mol ( x = 0; 0,125;
0,250; 0,375) menggunakan metode Chemical Solution Deposition dengan teknik
spin coating telah berhasil dibuat di atas substrat Si (100) tipe-p dan diputar pada
kecepatan 8000 rpm selama 60 detik. Proses annealing dimulai pada suhu ruang
dengan kelajuan 1,67°C/menit hingga mencapai suhu 850 °C dan ditahan selama
8 jam, dilanjutkan dengan proses pendinginan selama 12 jam hingga mencapai
suhu ruang. Ketebalan film dihitung menggunakan metode volumetrik dan
dihasilkan nilai ketebalan 2,0983 μm; 2,7977 μm; 3,4971 μm dan 3,6545 μm.
Hasil perhitungan menggunakan persamaan Cramer-Cohen diperoleh nilai
parameter kisi a = b = c, yaitu 3,975 Å; 3,981 Å; 4,073 Å dan 4,094 Å dengan
struktur kristal kubus. Hasil analisis menggunakan MAUD diperoleh visualisasi
struktur kristal kubus dengan parameter kisi 3,919 Å; 3,932 Å; 3,951 Å dan
3,956 Å. Nilai energi bandgap yang dianalisis menggunakan metode
Kubelka-Munk, yaitu 3,48 eV; 3,37 eV; 3,09 eV dan 3,05 eV. Fabrication of BaxSr1-xTiO3 thin films with various mol fractions (x = 0; 0,125; 0,250; 0,375) using the chemical solution deposition method with a spin coating technique has been successfully made on a p-type Si (100) substrate and rotated at a speed of 8000 rpm for 60 seconds. The annealing process begins at room temperature at a speed of 1,67°C/min until it reaches a temperature of 850°C and is held for 8 hours, followed by cooling process for 12 hours until it reaches room temperature. Film thickness was calculated using volumetric method and the results are 2,0983 μm; 2,7977 μm; 3,4971 μm and 3,6545 μm. The results of the calculation using Cramer-Cohen equation obtained that the lattice parameters a = b = c are 3,975 Å; 3,981 Å; 4,073 Å and 4,094 Å with cubic crystal structure. The results of the analysis using MAUD obtained a visualization of the crystal structure is cubic with lattice parameters are 3,919 Å; 3,932 Å; 3,951 Å and 3,956 Å. The values of bandgap energy that was analyzed using Kubelka-Munk method equation are 3,48 eV; 3,37 eV; 3,09 eV and 3,05 eV. |
| URI: | http://repository.ipb.ac.id/handle/123456789/109750 |
| Appears in Collections: | UT - Physics |
Files in This Item:
| File | Description | Size | Format | |
|---|---|---|---|---|
| Cover, Lembar Pengesahan, Prakata, Daftar Isi.pdf Restricted Access | Cover | 634.74 kB | Adobe PDF | View/Open |
| G74170004_Rizkiyah Khairun Ni'mah.pdf Restricted Access | Fullteks | 1.42 MB | Adobe PDF | View/Open |
| Lampiran.pdf Restricted Access | Lampiran | 945.73 kB | Adobe PDF | View/Open |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.