dc.description.abstractDurio Rind Pulp (DRP) cooking with soda, obtained from AA 20%, L/W 4:1, T 170oC for 4 hours without bleached. SWL give heat treatment in printer, feed five times, T 160oC then repulping. DRP and SWL mixed, the composition (w/w) 100/0, 75/25, 50/50, 25/75, and 0/100 with 3 different freeness, 300 CSF, 200 CSF, and 100 CSF. Dimensions and derivatives values DR all of which occupy fiber quality class II except felting power quality class III. While SWL occupies quality class III. Levels solubility of ethanol benzene, holocellulose, lignin, and α cellulose DR is 23%, 65.39 - 67.28%, 16.34 - 18.17%, 41.16 - 42.38%. While the level of solubility NaOH 1% of fiber DR > DRP 300 CSF > DRP 200 CSF > SWL. The mechanical properties of the sheets pulp mixture decreased with increasing composition of DRP. It is thought to because the DRP had higher levels of low weight polysaccharides and cellulose degradation is high. While the mechanical properties of SWL can be improved by beating.en
dc.subjectBogor Agricultural University (IPB)en
dc.subjectSorted White Ledger’s pulpen
dc.subjectDurio’s pulpen
dc.subjectBeatingen
dc.subjectPulp Compositionen
dc.subjectFreenessen
dc.titleSifat Kekuatan Pulp dari Campuran Pulp Daur Ulang dengan Pulp Kulit Buah Durianen
Appears in Collections:UT - Forestry Products

Files in This Item:
File SizeFormat 
E13afa.pdf
  Restricted Access
880.67 kBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.