Title: Analisis Sifat Fisis dan Mekanis Kayu Randu (Ceiba pentandra L. Gaertn.) Terpadatkan dengan Pra Perlakuan Delignifikasi Parsial
Other Titles: Analysis of Physical and Mechanical Properties of Densified Randu Wood (Ceiba pentandra L. Gaertn.) with Partial Delignification as Pre-treatment
Authors: Nugroho, Naresworo
Augustina, Sarah
Nurhasnah
Issue Date: 2024
Publisher: IPB University
Abstract: Kayu randu (Ceiba pentandra L. Gaertn.) termasuk jenis kayu cepat tumbuh dan berkerapatan rendah berkisar 0,21-0,28 g.cm-3. Hal ini membatasi pemanfaatan jenis ini khususnya untuk tujuan struktural. Peningkatan kualitas dan kekuatan kayu dapat dilakukan dengan menerapkan proses densifikasi. Efektivitas proses ini dapat ditingkatkan dengan memberikan pra perlakuan berupa delignifikasi parsial. Tujuan penelitian ini adalah menganalisa sifat fisis dan mekanis kayu randu terpadatkan dengan pra perlakuan delignifikasi parsial. Proses densifikasi diawali dengan penerapan pra perlakuan delignifikasi parsial menggunakan campuran CH3COOH dan H2O2 (1:1) pada konsentrasi 20%, dan 25%, serta akuades (0%), dilanjutkan dengan proses densifikasi pada suhu 150 °C dan 160 °C selama 30 menit. Hasil penelitian menunjukkan bahwa penerapan pra perlakuan delignifikasi parsial pada proses densifikasi mampu meningkatkan sifat fisis dan mekanis, serta stabilitas dimensi kayu randu terpadatkan, kecuali nilai T/R-rasio. Penggunaan suhu 150 °C dengan konsentrasi 25% merupakan perlakuan optimum pada kayu randu terpadatkan.
Randu wood (Ceiba pentandra L. Gaertn.) is a fast-growing wood species with a low density ranging from 0,21-0,28 g.cm-3. This limits the utilization of this species especially for structural purposes. Improving the quality and strength of wood can be done by applying densification process. The effectiveness of this process can be improved by applying partial delignification as pre-treatment. The purpose of this study was to analyze the physical and mechanical properties of densified randu wood with partial delignification as pretreatment. The densification process begins with the application of partial delignification as pretreatment using a mixture of CH3COOH and H2O2 (1:1) at concentrations of 20%, and 25%, as well as aquadest (0%), followed by the densification process at 150 °C and 160 °C for 30 minutes. The results showed that the application of partial delignification as pretreatment in the densification process was able to improve the physical and mechanical properties, as well as the dimensional stability of randu densified wood, except for the T/R-ratio value. The use of 150 °C temperature with 25% concentration is the optimum treatment in term of randu densified wood.
URI: http://repository.ipb.ac.id/handle/123456789/157809
Appears in Collections:UT - Forestry Products

Files in This Item:
File Description SizeFormat 
cover_E2401201033_af235266e401464aad823959f10648a3.pdfCover476.31 kBAdobe PDFView/Open
fulltext_E2401201033_27f455f3e7f44a64bbd4e95f35863a83.pdf
  Restricted Access
Fulltext869.75 kBAdobe PDFView/Open
lampiran_E2401201033_0763ccae82a2456bab9cc443233a9fef.pdf
  Restricted Access
Lampiran233.57 kBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.