Title: Pengaruh Perlakuan Pendahuluan pada Strand terhadap Sifat Fisis dan Mekanis Oriented Strand Board Kayu Sengon (Paraserianthes falcataria (L.) Nielsen)
Other Titles: Effect of Strand Pretreatment on Physical and Mechanical Properties of Oriented Strand Board from Sengon Wood (Paraserianthes falcataria (L.) Nielsen)
Authors: Febrianto, Fauzi
Noviyanti, Derisna
Issue Date: 2021
Publisher: IPB University
Abstract: Penelitian ini bertujuan mengevaluasi karakteristik OSB kayu sengon dengan perlakuan pendahuluan steam dan steam bilas NaOH 1%. Strand kayu sengon diberi perlakuan steam pada suhu 126 ℃ dengan tekanan 0,14 MPa selama 1 jam dan dilanjutkan dengan pembilasan NaOH 1%. Strand dicampur dengan perekat Phenol Formaldehyde (PF) pada konsentrasi 10%. Papan berukuran (30x30x0,9) cm3 disusun 3 lapis dengan kerapatan target 0,55 g.cm-3 dan nisbah lapisan 25:50:25. Pengujian sifat fisis dan mekanis mengacu pada standar JIS A 5908 (2003) yang hasilnya dibandingkan dengan standar CSA 0437.0 (Grade O-1). Hasil penelitian menunjukkan bahwa perlakuan pendahuluan strand memberikan pengaruh terhadap stabilitas dimensi OSB. Perlakuan steam bilas NaOH 1% menghasilkan OSB dengan sifat fisis yang lebih baik dari perlakuan steam tanpa perlakuan lanjutan. Namun, perlakuan steam dan steam bilas NaOH 1% tidak berpengaruh terhadap sifat mekanis OSB. Secara keseluruhan, karakeristik OSB pada setiap perlakuan pendahuluan mampu memenuhi standar CSA 0437.0 (Grade O-1), terkecuali pada beberapa parameter sifat mekanis.
The objectives of this research were to evaluated the characteristics of OSB from sengon wood with steam treatment and steam-treated followed by washing 1% NaOH. The sengon wood strand was treated with steam at a temperature of 126 ℃ with a pressure of 0,14 MPa for 1 hour and followed by washing with 1% NaOH. Strands were mixed with phenol formaldehyde (PF) adhesive at a concentration of 10%. Three layered of OSB was made with the size of (30x30x0,9) cm3, target density of 0,55 g.cm-3, and shelling ratio of 25:50:25. Testing of physical and mechanical properties of OSB refers to the JIS A 5908 (2003) standard and the results are compared with the CSA 0437.0 (Grade O-1) standard. The results show that the pretreatment of strand has an effect on the dimensional stability of OSB. The steam-treated follow by washing with 1% NaOH produce OSB with better physical properties than the steam without further treatment. However, the steam and steam-treated follow by washing with 1% NaOH has no effect on the mechanical properties of the OSB. Overall, the characteristics of OSB in each pretreatment met the CSA 0437.0 (Grade O-1) standard, prefix on some parameters of mechanical properties.
URI: http://repository.ipb.ac.id/handle/123456789/107563
Appears in Collections:UT - Forestry Products

Files in This Item:
File Description SizeFormat 
Cover.pdf
  Restricted Access
Cover572.8 kBAdobe PDFView/Open
SKRIPSI DERISNA FIX.pdf
  Restricted Access
Full Teks6.98 MBAdobe PDFView/Open
Lampiran.pdf
  Restricted Access
Lampiran217.41 kBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.